Application-first concrete fibre engineering[email protected] · WhatsApp +86 159 6543 3989
Technical Article

Post-Crack Creep in Fibre-Reinforced Tunnel Segments: What Designers and Producers Need to Verify

November 11, 2026

Fibre reinforced concrete creep in tunnel segments must be split into ordinary matrix creep, member behaviour before cracking and time-dependent response after cracking. A short-term residual-strength or full-scale segment test does not automatically prove sustained crack control. Designers need project load stages, crack-state assumptions, exposure and an accepted long-term model; producers must preserve the material and process represented by that evidence.

Three time-dependent questions must not be merged

Compression creep and shrinkage of the concrete matrix

These influence segment deformation, stress redistribution and restraint even before fibre bridging becomes active. The mix, humidity, temperature, age at loading and duration matter.

Long-term behaviour of an uncracked or partly cracked segment

Segment geometry, reinforcement, joints, ring interaction, handling and ground/load history determine whether and where cracking develops. This is a member-level problem, not a fibre property.

Post-crack creep of fibre-reinforced concrete

Once a crack is bridged, crack opening may evolve under sustained load through matrix compression creep, time-dependent fibre–matrix debonding/pull-out and, depending on fibre material, time-dependent deformation in the fibre itself. Pujadas et al. (2017) discusses these mechanisms in macro-synthetic FRC. They require a cracked-composite test and interpretation, not just a fibre tensile-strength value.

Why a five-minute beam test cannot answer a multi-year question

Standard short-term beam or panel tests characterise response under their specified loading procedure. They are valuable for quality and design parameters, but they do not expose a precracked specimen to sustained load for months, variable humidity, temperature or chemistry.

Likewise, a full-scale segment test can reveal load paths, local cracking and ultimate or service response for the tested configuration. It does not become a long-term post-crack creep result unless the test programme actually includes sustained cracked loading and the relevant environment.

The evidence chain should therefore separate:

Evidence Useful conclusion Long-term limit
Fibre TDS material and geometry identity no composite post-crack creep result
Short-term beam/panel test residual response or energy under the method no sustained-load evolution
Short-term full-scale segment test member response for tested configuration no automatic months/years extrapolation
Sustained precracked test time-dependent opening under defined load/environment limited to tested materials and conditions
Segment design model integrates project load stages and system behaviour depends on validated inputs and assumptions
Production QA shows approved process was followed does not validate the design model

What the Pujadas study does—and does not—show

The peer-reviewed study used 30 precracked beams, each 150 × 150 × 600 mm, under four-point bending sustained loading for five months. It included two environmental conditions and precrack openings of 0.25, 1.5 and 2.5 mm. The open manuscript records the programme in detail.

For the specific material series and conditions in that study, the reported creep coefficient for polymer-fibre-reinforced concrete was approximately twice that of the steel-fibre-reinforced concrete comparator. This is a study result—not a universal ratio for polypropylene, Conchip fibres or tunnel segments.

The following extrapolations would be unsupported:

  • treating 0.25, 1.5 or 2.5 mm as allowable segment crack widths;
  • treating five months as a design life;
  • applying the reported ratio to different fibres, matrices or environments;
  • applying beam results directly to ring capacity without a model;
  • concluding that all macro-synthetic FRC is unsuitable or that all steel FRC is superior.

The study’s proper use is to show why post-crack creep can be material- and condition-sensitive and why a long-term verification route may be needed.

Map every tunnel segment load stage

ITA Report No. 22 separates the important stages in segmental tunnel lining design. A project matrix should at least identify:

  • production, demoulding, storage and transport;
  • handling and erection;
  • TBM thrust and construction loads;
  • ring build, key insertion and joint contact;
  • tail-void grouting and early ground interaction;
  • service ground and groundwater actions;
  • local point or uneven contact;
  • long-term redistribution and environmental exposure.

For each stage, state whether cracking is expected or permitted, the duration of sustained action, the combination with shrinkage/temperature and what crack or deformation output the design controls.

Connect material, member and ring evidence

ITAtech’s design guidance for fibre-reinforced precast segments supports a project design route rather than a product-only conclusion. The useful hierarchy is:

  1. composite short-term residual response;
  2. sustained cracked response at the relevant load ratio and environment;
  3. member model and local details;
  4. short- and, where required, long-term member validation;
  5. ring/joint and construction-stage checks;
  6. production controls that reproduce the approved composite.

Short-term full-scale studies such as Liu et al. (2020) and Patel et al. (2023) are useful examples of segment-level comparison. They must not be presented as product-specific long-term proof when they did not test that product under sustained project conditions.

Define the sustained precracked test question

Where project risk requires long-term cracked-composite evidence, the responsible parties should agree:

  • fibre, matrix and production represented;
  • specimen geometry, notch or precracking method;
  • precrack opening and measurement method;
  • age and strength at precracking/loading;
  • sustained load level or ratio and how it relates to design;
  • temperature, humidity and any water/chemical exposure;
  • duration, reading schedule and interruption control;
  • creep/deformation definition and reporting units;
  • failure, instability and censoring rules;
  • number of specimens and variability treatment;
  • model calibration and acceptance criteria.

A published protocol can inform this plan, but project values should not be copied from another matrix or fibre.

Candidate Conchip information and the evidence gap

The current controlled TDSs for High Strength 48 and Wavy 48 identify both as 48 mm macro-synthetic fibres with 0.95 mm equivalent diameter, nominal tensile strength of at least 570 MPa, elongation below 30% and elastic modulus of at least 11 GPa. Each gives 4–8 kg/m³ as a starting trial range only and wet mixing of an additional 3–5 minutes after addition or until uniform dispersion is confirmed.

These documents do not provide project-specific post-crack creep data. They also do not establish segment crack width, sustained load ratio, member capacity, service life or approval. If either fibre enters a long-term segment design, the missing evidence must be resolved through project testing, justified external data or an accepted conservative model.

The producer’s role after the design route is approved

Long-term evidence only remains relevant if production reproduces the represented composite. The plant should link:

  • fibre product, TDS revision and lot;
  • actual dosage and dosing-device record;
  • approved mix and constituent lots;
  • fibre addition and mixing sequence;
  • batch, mould and segment ID;
  • curing and demoulding conditions;
  • companion specimens and test results;
  • deviations, quarantine and disposition.

A change in fibre, matrix, dosage, mixing, curing or specimen production may affect whether the original long-term evidence remains applicable. Define change-control authority in advance.

Long-term evidence checklist

  • Separate compression creep, uncracked member behaviour and post-crack creep.
  • Map production, construction and service load stages.
  • State crack-state and duration assumptions for each stage.
  • Identify the short-term composite parameter used by the design.
  • Decide whether sustained precracked evidence is required.
  • Represent the actual matrix, fibre, load ratio and environment.
  • Link beam evidence to the segment model without direct geometry extrapolation.
  • Validate critical member/ring behaviour at the level set by risk.
  • Lock production controls and change management.
  • Record residual uncertainties and responsible approval.

Frequently asked questions

1. What is post-crack creep in fibre-reinforced tunnel segments?

It is the time-dependent evolution of deformation or crack opening in cracked FRC under sustained action. It is distinct from ordinary concrete compression creep and from a short-term residual-strength test.

2. Does a standard residual-strength beam test prove long-term crack control?

No. It provides short-term response under its method. Long-term crack control needs sustained-load assumptions, environment, a suitable test or model and project acceptance.

3. Did the Pujadas study prove polymer FRC always creeps twice as much as steel FRC?

No. Approximately twice was reported for the study’s particular materials, specimens, precracks, load and environments. It must not be universalised to all polymers, products or segments.

4. Do High Strength 48 or Wavy 48 TDSs provide post-crack creep values?

No. They provide controlled fibre identity and starting trial/mixing information. Project-specific sustained cracked-composite evidence is a separate gap.

5. When is a project-specific long-term test most important?

It becomes more important when fibre bridging contributes materially under sustained service load, cracks remain open, consequences are high, the exposure is demanding or the model cannot be justified from applicable evidence.

Related technical guidance

Public sources and controlled documents

Next step

For a long-term evidence review, send the segment duty, load stages, crack assumptions, matrix, proposed fibre, exposure, short-term results and design model. Conchip can map the missing product and production evidence; the responsible designer retains model and acceptance authority.